Thu May 18 14:41:39 CST 2023
High temperature atomic ash bite bottom electrophoresis, is due to the atomic ash in the highly reactive reactive monomer has a very strong solvency, whether two-component self-drying primer or electrophoresis primer, if not fully cured that scraping atomic ash, the primer will be dissolved corrosion, the formation of irregular wrinkles, under the influence of temperature gas expansion, and the formation of bubbles, so before scraping high-temperature atomic ash.
High temperature atomic ash bites bottom electrophoresis, is due to the high activity reactive monomer in the atomic ash has a very strong solvency, whether two-component self-drying primer or electrophoresis primer, if not fully cured that scraping atomic ash, the primer will be dissolved corrosion, the formation of irregular wrinkles, under the influence of temperature gas expansion, and the formation of bubbles, so before scraping high temperature atomic ash.